49 C.F.R. § 192.489

Current through May 31, 2024
Section 192.489 - Remedial measures: Cast iron and ductile iron pipelines
(a)General graphitization. Each segment of cast iron or ductile iron pipe on which general graphitization is found to a degree where a fracture or any leakage might result, must be replaced.
(b)Localized graphitization. Each segment of cast iron or ductile iron pipe on which localized graphitization is found to a degree where any leakage might result, must be replaced or repaired, or sealed by internal sealing methods adequate to prevent or arrest any leakage.

49 C.F.R. §192.489