49 C.F.R. § 192.315

Current through November 30, 2024
Section 192.315 - Wrinkle bends in steel pipe
(a) A wrinkle bend may not be made on steel pipe to be operated at a pressure that produces a hoop stress of 30 percent, or more, of SMYS.
(b) Each wrinkle bend on steel pipe must comply with the following:
(1) The bend must not have any sharp kinks.
(2) When measured along the crotch of the bend, the wrinkles must be a distance of at least one pipe diameter.
(3) On pipe 16 inches (406 millimeters) or larger in diameter, the bend may not have a deflection of more than 11/2° for each wrinkle.
(4) On pipe containing a longitudinal weld the longitudinal seam must be as near as practicable to the neutral axis of the bend.