Wis. Admin. Code Department of Natural Resources NR 812.18

Current through December 30, 2024
Section NR 812.18 - Welding procedures

Plain end well casing pipe shall be welded watertight using welding procedures for plain end well casing pipe in accordance with the specifications in the American Welding Society manual AWS D10.12, "Guide for Welding Mild Steel Pipe." Well casing pipe to be welded shall conform to the specifications in s. NR 812.11(6). Pitless adapter connections to well casing pipe shall be made watertight in accordance with welding procedures in the American Welding Society manual AWS D1.1, "Structural Welding Code-Steel."

Wis. Admin. Code Department of Natural Resources NR 812.18

Cr. Register, January, 1991, No. 421, eff. 2-1-91; correction made under s. 13.92(4) (b) 6, Stats., Register July 2010 No. 655; CR 13-096: cr. (3) Register September 2014 No. 705, eff. 10-1-14; correction in numbering (1), (2) made under s. 13.92(4) (b) 1, Stats., Register September 2014.
Amended by, CR 18-095: r. and recr. Register June 2020 No. 774, eff. 7/1/2020

Copies of AWS manuals may be obtained directly from the American Welding Society's website at www.aws.org. Copies are also on file at the offices of the department and the legislative reference bureau.