Section 252:515-11-36 - Construction tests
(a) During liner construction, moisture and density tests shall be performed on each compacted lift at a rate of at least three per acre for each approximately six-inch compacted lift. A minimum of two tests shall be performed on the bottom and one on sideslope areas.
(b) One of the following methods shall be used:
(1) nuclear density method using (ASTM D2922), to include the conventional oven drying method (ASTM D2216) performed on every ten samples;
(2) drive-cylinder method (ASTM D2937);
(3) rubber balloon method (ASTM D2167);
(4) sand-cone method (ASTM D1556);
(5) microwave drying method (ASTM D4643); or
(6) conventional oven drying method (ASTM D2216).